My pH looked correct before starting (4.5 or 4.6) and at the end of the dye session is now 5.0.  My guess is this won't exhaust very well either.

Coolsticks (not verified)

You may want to recycle the metal parts of a belt from the thrift store.

pjdoney (not verified)

My results look to be about the same old, same old color.  I think a little more dye did exhaust this time but there's still a lot of red in the water.  My guess is that in trying to get the high temp that water surrounding the jar would splash into the jar with skein and dye.  Knowing that my water has a pH of 5.3, I am assuming that is the culprit for the raising of my pH level to 5.0 from 4.5/ 4.6.

I could try putting aluminum foil over the top of the dye jar once the water bath gets more active.  I would prefer waiting to do that until I put the lid on the pot because of fussing but that might not be an option. 

I can send you a picture but honestly, you've already seen very similar results.  Do you want me to post on the spreadsheet?

pjdoney (not verified)

Share the misery....before and after pH pictures:

 

Made my new dye bath using 5 L water, 1/2 tsp A. Set, 1/4 tsp Sodium acetate, and 10 gr Glauber salt.  pH was lowered to approx. 4.5 using acetic acid.  Soaked 5 gr skein in water, then soaked in dye bath (10 min), removed skein, put 2.25 mL Olive Green in jar and replaced skein and let it sit (10 min).  In just over an hour temp was raised from 19 C to 94 C with a dwell time of 1 hour (dunking every few minutes).  Cool down of several hours, rinse, etc.

Jeff and I are wondering about making an e-collar out of aluminum foil so I can dunk but hopefully keep out lively water splashes.  That would also allow for me to monitor its temp more easily.

pjdoney (not verified)

I did take the pH before and after the other two previous cooking times.  They were about 4.6 at the beginning and end of processing.

So, you want me to make a third new dyebath using distilled water.  I used fresh dyebath this morning after throwing out the orignal batch.  I don't have the sodium hexametaphosphate but can order some in.  I will test the pH of the dye bath after adding Glaubers (test), sodium acetate (test), and A. Set (test).  I should also test the pH of the dyebath before I put the wool skein in.

Did I miss anything?

Cameron T-B (not verified)

These "threads" of conversation are getting more esoteric by the minute - but fun! Thanks.

 

 

pjdoney (not verified)

5L distilled water 5.0 pH

1/4 tsp/ 2.5L A. Set  4.9 or 4.8 pH

1/4 tsp sodium acetate/ 5L  5.3? pH

2 gr/ L Glauber salt  5.6 or 5.7? pH

12 mL 5% acetic acid  4.5 pH

I measured the pH of these in the order written.  Some of the pH colors were very hard to tell so I have indicated my uncertainty (gotta find my digital pH meter!).

Here is a link to our utility company's report on our water:

http://www.csu.org/residential/services/water/wqr/item6292.pdf

Approximately 75% of our water comes from mountain streams.  "The majority of this raw water is transferred to our city through pipelines that help to protect it from contamination, such as herbicides, pesticides, heavy metals, and other chemicals."

In addition to this water, we also use local surface and ground water sources (slopes of Pikes Peak, creeks, watershed, wells on three different aquifers) and treated surface water that is routed through a river.

Here is a link to the Detected Contaminant Table:

http://www.csu.org/residential/services/water/wqr/item6298.pdf

Copper is listed at 1.3 ppm and lead is 0 ppb.

As far as I know, we have soft water.

Now, your previous comment that:

"Sometimes the addtion of the wool or dye changes the pH and that is a problem if the pH has already risen to 5.0 before you start heating, that would cause less exhaust."   - I should put my wool in the 300 mL dye bath and check the pH right away and let it sit for 10 minutes.  Take the skein out, add 2.25 mL of Olive dyestock, put skein back in, and measure the pH again, and let skein sit for 10 minutes.  If it is up to pH 5, should I add small amounts of acetic acid to the 300mL dyebath/ plus dye?

 

Thanks, Karren, for your help.  I haven't pulled any of my hair out...yet...

steve104c (not verified)

To me, and this is just a thought, it looks like when you started with the scrap weft to get the warp threads separated, the weft wasn't beaten down enough. When I beat down my weft, the weft ends up really tight and the warp threads separate nicely.  I,m at work right now and can't send you a close-up pic. of my rugs where you can see how tight I beat the weft. Thats why I love my Glimakra, I can beat the weft really really hard. I'm just a beginner and I'm not really qualified to give advice, so this is "just a thought" ..........Steve.

jordanj (not verified)

Us guys are excited for you! Let us know how it goes and post a picture of your booth so we can see all the colors!

Katie Lacewell (not verified)

Thanks, Kerstin.  I'll try putting the locking pins in half way and removing the lamms not being used.

Katie