In the throes of the Christmas weaving marathon...

Wove wool scarf.  My wife wanted it in "spice brown" from the Cushing Dye list.  OK, fine.  I warned her that sometimes the color is not accurate.  

Dyed her scarf last night, and it came out a very nice shade of ...

GREY.

(with a hint of brown).

What the heck did I do wrong?  Fortunately, she likes the color, but I have another scarf to dye for a friend and don't want the same trouble.  I thought I followed the instructions...

 

Allen

Comments

Badfaerie (not verified)

I haven't used Cushings in a while, but it is my experience that with some dyes the colors "strike" at different temperatures. If the color you are using is a mix of other colors, which spice brown sounds like it would be, you might have hit the temperature for the only some of the colors in it.

Also check what you are dying it in, metal pots can mordant the water and alter the colors. Spinning oils/sizing can affect how the dyes strike. The color of the wool to start with can change things... the amount of dye/acid/dye assists... there are a lot of variables.

apw1970 (not verified)

I was wondering the same thing, but didn't think of the pot material.  I use stainless steel, so that shouldn't mordant the fibers.  I wonder if the problem could be with the fact that I didn't scour the scarf first (thought it would felt... stupid thought stupid thought...).  I have read about the different temp/color curve thing too, and that's why I let the scarf simmer a long time.  I have two more to do and will test scour and dye a a sample first before I put the next scarf in...

laurafry

Scouring by and of itself won't full wool - scouring is just the removal of oils/dirt using soap/detergent.  It is moist agitation that may cause fulling.  (Not all wools full.)

cheers,

Laura

bvfrenchknitter (not verified)

Stainless Steel is OK.  You would need to make sure all oils are out of the wool.  I like Dawn dish detergent and hot water.  You can use hot water as long as you use water that is always the same temperature for a wash and rinse.  A change in temperature causes felting and as is said above, agitation. 

When you dye you need to use a water bath, with vinegar and bring the temperature up after you add the dye, dissolve it and the item to be dyed.  It is stirred and dyed till the water goes clear, if you have the proper amount of dye.  If you have far more dye than you need you might not have the water go clear when you get the color you want.  You want the temperature to come up to a boil, then reduce and simmer for 30 - 40 minutes.  According to the Cushing instructions different components will strike (dye a particular color) at different temperatures so that might be causing your problem (since brown is a mixture of colors).  After the item is the color you want take out, let it come to room temperature and then wash.  Oh, the amount of dye is also a function of the amount of fabric/yarn being dyed.  My favorite resource for dyes is Pro Chemical but their acid dyes aren't Cushing so I looked at the Cushing instructions since I've used a lot of acid dyes but never Cushing.  I use Sabraset dyes myself, but all the acid dyes are similar I think. 

You can try to dye the scarf again and you can also put a little of the dye mix on a bit of unwoven yarn, wrap in saran wrap and then steam it for 10 minutes or so in saran wrap so it is waterproof to get an idea of the color you will get.  You have to make sure to use dedicated pans and stuff and never use them for food again but samples and testing will give you an idea.  You can also mix acid dyes and get different colors. 

The only other thing that occurs to me is are you sure it is pure wool?  Acid dyes only work for wool, silk and nylon.  If you are dealing with a blend the dye would only work on the wool/nylon and silk.  I've dyed wool/cotton blends and gotten similar results.

 

Submitted by Anonymous (not verified) on